Skip to main content
← Notes from the Assembly Floor

X-Ray Inspection on Circuit Board Assemblies: What It Finds That Nothing Else Can

Allendale Electronics November 20, 2026

X-Ray Inspection on Circuit Board Assemblies: What It Finds That Nothing Else Can

Some solder joints sit where nobody can look at them. On a ball grid array, the connections are a grid of solder balls pressed between the underside of the part and the board. Micro-BGAs, QFNs and LGAs follow the same layout, with their terminations tucked under the body of the component. Once the part is placed and reflowed, the package covers every joint it made.

That leaves no line of sight. A technician with a loupe sees the edge of the package and the board around it. A high-resolution camera sees the same edge from a better angle. The joint stays behind the component body, and the limit comes from geometry, so training and pixel count do not change it.

PCB X-ray inspection exists for this reason. X-ray inspection of PCB assembly uses an X-ray source and a detector, and the image forms from how much radiation each material absorbs. Solder is dense, so it absorbs a lot and shows up dark. Silicon, fibreglass and plastic let more through and show up light. The result is a picture of the solder inside and beneath the package, where the shape, volume and internal condition of each joint can be read.

Where AOI Does Its Job and Where It Runs Out

Automated optical inspection is the workhorse of the SMT line. A camera scans the board and checks that each component is present, that its polarity is right, that it sits close to its pads, and that the visible solder fillets on leaded and standard SMT parts look correct. At Allendale, every surface-mounted board passes AOI before it moves further down the line.

For anything the camera can see, AOI and X-ray overlap. Both can catch open circuits, solder bridges and shorts, insufficient or excess solder, and parts that are missing or misaligned. The side-by-side comparison of AOI and X-ray defect detection shows where the overlap ends. Solder voids, general internal solder quality, and shorts or open connections under a BGA belong to X-ray alone.

The dividing line follows the light. A camera records the surface it can reach, so a fillet on a gull-wing lead is fully in view. A ball under a package is out of view, and so is a void inside a joint that looks perfect from the side. Automated X-ray inspection of a PCB picks up at that boundary, since the beam passes through the package and the board and records what the solder looks like inside.

Reading the two methods this way keeps expectations accurate. AOI covers the visible surface of every board, and X-ray covers the hidden joints that the surface view cannot reach.

What X-Ray Reveals Under the Package

BGA solder joint inspection comes down to a handful of conditions that an X-ray image makes visible:

  • Voids: air pockets trapped in the solder when flux outgasses during reflow.
  • Bridging: solder that links two neighbouring balls and creates a short under the package.
  • Insufficient or excess solder: a ball that looks too small or too large against its neighbours.
  • Misalignment: a ball sitting off centre on its pad.
  • Open joints: a ball that never wet to the pad and left no connection.

Voids get the most attention because every reflowed joint carries some. A small void does little harm. A large one shrinks the area that carries current and heat, and it gives a crack a place to start when the board sees vibration or thermal cycling. That is why a void reading is judged against a limit and never in isolation. The commonly cited IPC-A-610 limit of roughly 25% void area per individual solder ball is one such yardstick, and older revisions are referenced at about 30%. Class 3 work is commonly cited at tighter limits of under 15% for an individual ball and under 20% cumulative, against under 25% and 30% for Class 2.

Bridging, shortage and misalignment matter for a simpler reason. A bridge under a package is a short that no one can see until the board is powered, and a ball that is off its pad carries less load than its neighbours.

Fine pitch raises the demand on the equipment. BGAs below 0.4 mm pitch typically need 2 to 3 μm resolution at 500 to 1500x magnification to image clearly, which is a job for a dedicated X-ray system and out of reach for general-purpose imaging.

Barrel Fill on Through-Hole and Mixed-Technology Boards

BGAs are the best-known reason for X-ray, and through-hole boards have their own. A plated through-hole joint depends on solder filling the barrel, the copper-plated hole that runs through the board. IPC-A-610 asks for a minimum of 75% vertical fill for both Class 2 and Class 3 assemblies. Class 2 allows a narrow exception of 50% fill on components with 14 or more leads that meet specific conditions for visible lead and wetting. The difference between the classes is covered in more detail in our post on IPC Class 2 and Class 3.

Fill depth matters because the solder inside the barrel carries the mechanical load and the thermal and electrical path. A joint that is only partly filled has less of each. Pins on connectors and heavy parts feel the stress of handling, vibration and temperature swings, so a half-filled barrel is where a field failure begins.

The trouble is that the top and bottom of a through-hole joint can look fine while the barrel holds a gap partway up. Of the common PCB inspection methods, visual checks and AOI read the surfaces, and X-ray reads the volume. That makes X-ray the method that confirms fill on boards where mixed technology puts through-hole parts beside SMT parts.

Where X-Ray Fits in a Real Quality Process

X-ray works best as a targeted step on a line where every board is already optically inspected. Shops deploy it as sample-lot verification on hidden-joint packages, and as a diagnostic tool when a board fails functional test or shows a suspect reading elsewhere. AOI runs on every board as a matter of course. X-ray is reserved for what AOI cannot reach and for cases that call for a deeper look.

Allendale's process follows that pattern. Every surface-mounted board passes AOI, which scans for missing, incorrect or misplaced components. Our QA department uses a GlenBrook X-ray system to verify solder joints that cannot be checked visually, including BGAs and other hidden connections, and it samples assembly processes directly. That matters on a line that places micro-BGAs at 0.4 mm pitch, where the joints under the part are exactly the ones the camera cannot see.

Sampling gives a process-level answer. When the sampled joints show healthy fill, tight void readings and clean alignment, the reflow profile and placement are doing their jobs. When a reading drifts, the finding feeds back into the process before more boards are built.

X-ray also has a boundary of its own. It shows the shape and internal condition of solder, and it cannot detect electrical or logic faults. A joint can look perfect on X-ray and still sit under a dead component, and a good-looking joint can hold a weak metallurgical bond. Functional and electrical testing remain the methods that answer those questions, and each layer covers a different part of the picture.

One Layer in a Larger Quality Process

X-ray inspection sits inside a quality system built around IPC-A-610 and J-STD-001 workmanship standards, technicians trained in-house, and ESD-controlled handling of every material. Readers who want the full picture of how a build is verified from start to finish will find it on our quality process page, and those weighing an assembly partner can see the equipment behind it on our services page. If you have a board with hidden-joint packages, send us your files through Request a Quote and we will review them and come back with a clear, considered quote.

Have a board you'd like us to look at?

Send your files and we'll review them for manufacturability as part of the quote. Every build is inspected to IPC-A-610.

Request a quote